Co、Si共掺杂调控Ni-Mn-Ti合金马氏体相变、磁性能和力学性能的第一性原理研究 |
| 刘丹, 白静, 章羽, 郭珂良, 刘新, 左良 |
|
First-Principles Study on the Regulation of Martensitic Transformation and Magnetic and Mechanical Properties of Ni-Mn-Ti Alloy via Co and Si Codoping |
| LIU Dan, BAI Jing, ZHANG Yu, GUO Keliang, LIU Xin, ZUO Liang |
| 图4 Ni2 - x Co x Mn1.5 - y Si y Ti0.5 (0 ≤ x ≤ 0.625,y = 0.125和0.25)合金奥氏体与马氏体体积差(ΔV) |
| Fig.4 Volume change (ΔV) between austenite and martensite for Ni2 - x Co x Mn1.5 - y Si y Ti0.5 (0 ≤ x ≤ 0.625, y = 0.125 and 0.25) alloys |
|