Cu/Ta纳米双层膜拉伸变形及Al、W原子掺杂对其变形影响的分子动力学模拟 |
| 石腾龙, 陈娟, 赵彬, 史俊勤 |
|
Molecular Dynamics Simulations of Tensile Deformation of Cu/Ta Nano-Bilayer Films and the Effect of Al and W Atoms Doping on the Deformation |
| SHI Tenglong, CHEN Juan, ZHAO Bin, SHI Junqin |
| 图12 各模型初始时刻内部缺陷示意图及沿Z方向拉伸时位错结构产生示意图 |
| Fig.12 Schematics of internal defects at the initial strain (ε = 0) (a1-c1) and dislocation structure generation during stretching along the Z direction (a2-c2) for Cu/Ta (a1, a2), Cu95Al5/Ta (b1, b2), and Cu95W5/Ta (c1, c2) bilayer film models (a2) ε = 0.042 (b2) ε = 0.030 (c2) ε = 0.014 |
|