Cu/Ta纳米双层膜拉伸变形及Al、W原子掺杂对其变形影响的分子动力学模拟 |
| 石腾龙, 陈娟, 赵彬, 史俊勤 |
|
Molecular Dynamics Simulations of Tensile Deformation of Cu/Ta Nano-Bilayer Films and the Effect of Al and W Atoms Doping on the Deformation |
| SHI Tenglong, CHEN Juan, ZHAO Bin, SHI Junqin |
| 图7 Cu/Ta、Cu95Al5/Ta和Cu95W5/Ta双层膜沿X方向拉伸过程中不同应变下的位错结构 |
| Fig.7 Dislocation structures of Cu/Ta (a-c), Cu95Al5/Ta (d-f), and Cu95W5/Ta (g-i) bilayer films at different strains during stretching process along X direction (a) ε = 0.063 (b) ε = 0.169 (c) ε = 0.260 (d) ε = 0.060 (e) ε = 0.175 (f) ε = 0.260 (g) ε = 0.050 (h) ε = 0.170 (i) ε = 0.260 |
|