Cu/Ta纳米双层膜拉伸变形及Al、W原子掺杂对其变形影响的分子动力学模拟 |
| 石腾龙, 陈娟, 赵彬, 史俊勤 |
|
Molecular Dynamics Simulations of Tensile Deformation of Cu/Ta Nano-Bilayer Films and the Effect of Al and W Atoms Doping on the Deformation |
| SHI Tenglong, CHEN Juan, ZHAO Bin, SHI Junqin |
| 图4 Cu95Al5/Ta双层膜沿X方向拉伸过程中不同应变下的晶体结构 |
| Fig.4 Crystal structures of Cu95Al5/Ta bilayer films at different strains during stretching along X direction (a) ε = 0.060 (b) ε = 0.070 (c) ε = 0.100 (d) ε = 0.155 (e) ε = 0.175 (f) ε = 0.260 |
|