Cu/Ta纳米双层膜拉伸变形及Al、W原子掺杂对其变形影响的分子动力学模拟 |
| 石腾龙, 陈娟, 赵彬, 史俊勤 |
|
Molecular Dynamics Simulations of Tensile Deformation of Cu/Ta Nano-Bilayer Films and the Effect of Al and W Atoms Doping on the Deformation |
| SHI Tenglong, CHEN Juan, ZHAO Bin, SHI Junqin |
| 图3 Cu/Ta双层膜沿X方向拉伸过程中不同应变下的晶体结构 |
| Fig.3 Crystal structures of Cu/Ta bilayer films at different strains during stretching along X direction (ε—strain. Dashed lines indicate the interfaces between different structures, the same below) (a) ε = 0.063 (b) ε = 0.066 (c) ε = 0.085 (d) ε = 0.163 (e) ε = 0.169 (f) ε = 0.260 |
|