钢包静置过程夹杂物去除的工业试验与数值模拟 |
| 段豪剑, 谢忠研, 李占魁, 徐学军, 黄财德, 温瀚, 张立峰 |
|
Industrial Trial and Numerical Simulation of Inclusion Removal During Ladle Holding Period |
| DUAN Haojian, XIE Zhongyan, LI Zhankui, XU Xuejun, HUANG Caide, WEN Han, ZHANG Lifeng |
| 图8 钢包静置过程中直径为100 μm的夹杂物在钢液中的运动和去除 |
| Fig.8 Motions and removals of 100 μm inclusions in the molten steel during ladle holding time for 100 s (a), 600 s (b), and 1800 s (c) |
|