钢包静置过程夹杂物去除的工业试验与数值模拟
段豪剑, 谢忠研, 李占魁, 徐学军, 黄财德, 温瀚, 张立峰

Industrial Trial and Numerical Simulation of Inclusion Removal During Ladle Holding Period
DUAN Haojian, XIE Zhongyan, LI Zhankui, XU Xuejun, HUANG Caide, WEN Han, ZHANG Lifeng
图1 钢包吹氩密封成分调整(CAS)精炼的工艺操作和取样记录示意图
Fig.1 Schematic of operations and sampling processes during composition adjustment by sealed argon bubbling (CAS) refining (A represents adding 51 kg FeAl and 135 kg Al; B represents adding 51 kg high carbon FeMn, 526 kg middle carbon FeMn, and 48 kg FeAl; C represents adding 80 kg FeAl)