流动海水中多重应力耦合作用下B10 Cu-Ni合金的微观结构演变与动态失效机制
李瑞雪, 周晨曦, 杨慧敏, 雍兴跃, 刘景军

Microstructural Evolution and Dynamic Failure Mechanism of B10 Cu-Ni Alloy Under Multiple Stress Coupling in Flowing Seawater
LI Ruixue, ZHOU Chenxi, YANG Huimin, YONG Xingyue, LIU Jingjun
图8 压力(4.0 MPa、0 m/s)/流速(0.1 MPa、4 m/s)单一因素与耦合因素作用(4.0 MPa、4 m/s)条件下B10seg合金的迁移-溶解过程、腐蚀动力学参数及电荷密度分布
Fig.8 Migration-dissolution processes, corrosion kinetics parameters, and charge density distributions of B10seg alloy under the effect of pressure (4.0 MPa, 0 m/s)/flow velocity (0.1 MPa, 4 m/s) as single factors and coupled factors (4.0 MPa, 4 m/s)
(a, b) migration dissolution of Cu (a) and Ni (b) atoms under single/coupled mechanical conditions in B10seg alloy model
(c) comparisons of corrosion rate constant of B10seg alloy model
(d) surface energies of B10seg alloy model
(e) vacancy energies of B10seg alloy model
(f) work functions of B10seg alloy model
(g-i) charge density distributions of B10seg alloy model under 4.0 MPa (g), at 4 m/s (h), and under 4.0 MPa and at 4 m/s (i)