流动海水中多重应力耦合作用下B10 Cu-Ni合金的微观结构演变与动态失效机制
李瑞雪, 周晨曦, 杨慧敏, 雍兴跃, 刘景军

Microstructural Evolution and Dynamic Failure Mechanism of B10 Cu-Ni Alloy Under Multiple Stress Coupling in Flowing Seawater
LI Ruixue, ZHOU Chenxi, YANG Huimin, YONG Xingyue, LIU Jingjun
图7 4.0 MPa压力条件下,海水流速为1~5 m/s时B10seg合金的迁移-溶解过程,腐蚀速率常数与质量损失的对比;单一压力(4.0 MPa、0 m/s)/流速(0.1 MPa、4 m/s)及耦合因素(4.0 MPa、4 m/s)作用时B10合金表面腐蚀形貌的SEM像、XRD谱及(111)晶面的微应变和位错密度分析
Fig.7 Migration-dissolution process of B10seg alloy at 4.0 MPa with seawater flow velocities of 1-5 m/s, and the corrosion behavior of B10 alloy under the individual effects of pressure (4.0 MPa, 0 m/s) and flow velocity (0.1 MPa, 4 m/s) versus coupled effect (4.0 MPa, 4 m/s)
(a, b) migration-dissolution processes of B10seg-Cu (a) and B10seg-Ni (b) under 4.0 MPa pressure and different flow rates
(c) comparisons of corrosion rate constant and mass loss at different flow rates under 4.0 MPa
(d-f) SEM images of the surface corrosion morphology of the B10 alloy under 4.0 MPa (d), at 4 m/s (e), and under 4.0 MPa and at 4 m/s (f)
(g) XRD patterns of B10 alloy
(h) microstrains of (111) crystal plane in B10 alloy
(i) dislocation densities of B10 alloy