流动海水中多重应力耦合作用下B10 Cu-Ni合金的微观结构演变与动态失效机制
李瑞雪, 周晨曦, 杨慧敏, 雍兴跃, 刘景军

Microstructural Evolution and Dynamic Failure Mechanism of B10 Cu-Ni Alloy Under Multiple Stress Coupling in Flowing Seawater
LI Ruixue, ZHOU Chenxi, YANG Huimin, YONG Xingyue, LIU Jingjun
图6 常压条件下海水流速为1~5 m/s时B10合金表面腐蚀形貌的SEM像,XRD谱,(111)晶面的微应变和位错密度;B10seg合金的迁移-溶解过程,腐蚀速率常数与质量损失对比及腐蚀动力学参数分析
Fig.6 Corrosion behaviors of alloys under atmospheric pressure (0.1 MPa) at various seawater flow rates (1-5 m/s) (a1-a5) SEM images of B10 alloy under atmospheric pressure with seawater flow rates of 1 m/s (a1), 2 m/s (a2), 3 m/s (a3), 4 m/s (a4), and 5 m/s (a5) (b) XRD patterns of B10 alloy (c) microstrains of (111) crystal plane in B10 alloy (d) dislocation densities of B10 alloy (e) B10seg-Cu migration-dissolution process (f) B10seg-Ni migration-dissolution process (g) comparisons of corrosion rate constant and mass loss at different flow rates (h) relationship between surface energy and flow rate of B10seg alloy model (i) vacancy energies of B10seg alloy model (j) work functions of B10seg alloy model