流动海水中多重应力耦合作用下B10 Cu-Ni合金的微观结构演变与动态失效机制 |
| 李瑞雪, 周晨曦, 杨慧敏, 雍兴跃, 刘景军 |
|
Microstructural Evolution and Dynamic Failure Mechanism of B10 Cu-Ni Alloy Under Multiple Stress Coupling in Flowing Seawater |
| LI Ruixue, ZHOU Chenxi, YANG Huimin, YONG Xingyue, LIU Jingjun |
| 图5 不同海水压力下B10seg合金/海水界面溶剂化模型的建立,合金表面H2O分子的密度分布,模拟不同压力下H2O分子对合金中表面原子溶解影响的示意图模型,合金的表面能和功函数,海水压力对Helmboltz层影响的示意图,压力作用下原子的迁移-溶解过程及腐蚀速率常数与质量损失的对比 |
| Fig.5 Establishment of the solvation model at the B10seg alloy/seawater interface under different seawater pressures (a), density distributions of H2O molecule on the alloy surface (b), schematic model for simulating the effect of H2O molecules on the dissolution of surface atoms in alloys under different pressures (c), surface energy (d), work function (e), schematic of the influence of seawater pressure on the Helmholtz layer (OHP—outer Helmholtz plane) (f), Cu (g) and Ni (h) atomic migration-dissolution processes under different pressures, and comparisons of corrosion rate constant and mass loss under different pressures (i) |
|