流动海水中多重应力耦合作用下B10 Cu-Ni合金的微观结构演变与动态失效机制 |
| 李瑞雪, 周晨曦, 杨慧敏, 雍兴跃, 刘景军 |
|
Microstructural Evolution and Dynamic Failure Mechanism of B10 Cu-Ni Alloy Under Multiple Stress Coupling in Flowing Seawater |
| LI Ruixue, ZHOU Chenxi, YANG Huimin, YONG Xingyue, LIU Jingjun |
| 图2 B10 Cu-Ni合金不同晶面的快速Fourier变换(FFT)、逆快速Fourier变换(IFFT)及应变水平分析 |
| Fig.2 Fast Fourier transforms (FFT), inverse fast Fourier transforms (IFFT), interplanar spacings, and strain level analyses of different crystal planes of B10 Cu-Ni alloy (The color scale bars indicate strains: red-to-yellow for tensile strain, green-to-blue for compressive strain; white boxes mark tensile-compressive stress concentration zones) (a1-a3) FFT and IFFT on the (111) (a1), (200) (a2), and (220) (a3) crystal planes, along with their corresponding interplanar spacing line profiles (b1-b3) x-direction strain (εxx ) (b1), xy-direction strain (εxy ) (b2), and y-direction strain (εyy ) (b3) on the (111) crystal plane (c1-c3) εxx (c1), εxy (c2), and εyy (c3) on the (200) crystal plane (d1-d3) εxx (d1), εxy (d2), and εyy (d3) on the (220) crystal plane |
|