Mn / N比对22%Cr节Ni型双相不锈钢多道次焊接热影响区组织和力学性能的影响
郭孟雨, 杨银辉, 高梓豪, 曹建春, 吴诗裕, 陈晓雨

Effect of Mn / N Ratio on the Microstructure and Mechanical Properties of Multi-Pass Welding HAZ of 22%Cr Low Nickel Type Duplex Stainless Steel
GUO Mengyu, YANG Yinhui, GAO Zihao, CAO Jianchun, WU Shiyu, CHEN Xiaoyu
表1 双相不锈钢试样的化学成分及Mn / N比
Table 1 Chemical compositions and Mn / N ratios of duplex stainless steel (DSS) samples
Steel No.Mass fraction / %Mn / N ratio
CSiMnSPCrNiMoCuNFe
DSS10.0130.160.520.0090.00622.395.512.640.140.17Bal.3.06 (2205 steel)
DSS20.0040.201.960.0040.00722.061.322.720.110.52Bal.3.77
DSS30.0110.118.010.0090.00722.521.372.690.140.47Bal.17.80
DSS40.0110.1114.510.0060.00522.491.342.700.140.22Bal.65.91