Mn / N比对22%Cr节Ni型双相不锈钢多道次焊接热影响区组织和力学性能的影响 |
| 郭孟雨, 杨银辉, 高梓豪, 曹建春, 吴诗裕, 陈晓雨 |
|
Effect of Mn / N Ratio on the Microstructure and Mechanical Properties of Multi-Pass Welding HAZ of 22%Cr Low Nickel Type Duplex Stainless Steel |
| GUO Mengyu, YANG Yinhui, GAO Zihao, CAO Jianchun, WU Shiyu, CHEN Xiaoyu |
| 图13 DSS1~DSS4试样多道次焊接HAZ冲击断口夹杂物形貌、粒径统计和EDS分析结果 |
| Fig.13 Morphologies (a, d, g, j), particle size distributions (b, e, h, k), and EDS results (c, f, i, l) of inclusions in multi-pass welding HAZ impact fractures of DSS1 (a-c), DSS2 (d-f), DSS3 (g-i), and DSS4 (j-l) samples (σ—standard deviation) |
|