Mn / N比对22%Cr节Ni型双相不锈钢多道次焊接热影响区组织和力学性能的影响 |
| 郭孟雨, 杨银辉, 高梓豪, 曹建春, 吴诗裕, 陈晓雨 |
|
Effect of Mn / N Ratio on the Microstructure and Mechanical Properties of Multi-Pass Welding HAZ of 22%Cr Low Nickel Type Duplex Stainless Steel |
| GUO Mengyu, YANG Yinhui, GAO Zihao, CAO Jianchun, WU Shiyu, CHEN Xiaoyu |
| 图7 DSS4试样经多道次焊接热循环后HAZ的STEM像、SAED花样及EDS分析 |
| Fig.7 STEM images, SAED patterns, and EDS result of HAZ for DSS4 sample after multi-pass welding (a-c) two-phase morphology distributions (a) and SAED patterns of austenite (b) and ferrite (c) (d) dislocation tangles near γ/δ interfaces (e) reformed austenite morphology in two phases (f-h) distribution of σ-phase precipitates and the amplified morphology (inset) (f), SAED pattern (g), and corresponding compositions (h) |
|