Mn / N比对22%Cr节Ni型双相不锈钢多道次焊接热影响区组织和力学性能的影响
郭孟雨, 杨银辉, 高梓豪, 曹建春, 吴诗裕, 陈晓雨

Effect of Mn / N Ratio on the Microstructure and Mechanical Properties of Multi-Pass Welding HAZ of 22%Cr Low Nickel Type Duplex Stainless Steel
GUO Mengyu, YANG Yinhui, GAO Zihao, CAO Jianchun, WU Shiyu, CHEN Xiaoyu
图5 DSS1和DSS2试样经多道次焊接热循环后HAZ组织的STEM像和选区电子衍射(SAED)花样
Fig.5 STEM image and SAED patterns of HAZ for DSS1 and DSS2 samples after multi-pass welding
(a-c) morphology (a), SAED pattern of γ (b), and dislocation distribution (c) of DSS1 sample
(d-i) morphology (d) and corresponding SAED patterns of γ and δ phases (e, f), dislocation distribution near γ/δ interface (g), and distribution of Cr2N precipitates (h) and corresponding SAED pattern (i) of DSS2 sample (Inset in Fig.5h is locally enlarged view)