晶粒尺寸与晶体取向对CrCoNi中熵合金孪晶界疲劳开裂行为的影响
王玉洁, 李琳琳, 张振军, 张哲峰

Effects of Grain Size and Crystallographic Orientation on Fatigue Cracking at Twin Boundaries in CrCoNi Medium-Entropy Alloy
WANG Yujie, LI Linlin, ZHANG Zhenjun, ZHANG Zhefeng
图6 不同晶粒尺寸CrCoNi MEA样品在0.4%总应变幅下疲劳后孪晶界两侧疲劳形貌特征
Fig.6 Surface deformation features in FG (a) and CG (b) CrCoNi MEA specimens fatigued at a total strain amplitude of 0.4%; and height (h) fluctuations of slip bands for FG (c) and CG (d) specimens along the arrows in Figs.6a and b, respectively