晶粒尺寸与晶体取向对CrCoNi中熵合金孪晶界疲劳开裂行为的影响
王玉洁, 李琳琳, 张振军, 张哲峰

Effects of Grain Size and Crystallographic Orientation on Fatigue Cracking at Twin Boundaries in CrCoNi Medium-Entropy Alloy
WANG Yujie, LI Linlin, ZHANG Zhenjun, ZHANG Zhefeng
图1 疲劳样品示意图
Fig.1 Schematic of fatigue specimen (unit: mm)