流动海水中多重应力耦合作用下B10 Cu-Ni合金的微观结构演变与动态失效机制 |
| 李瑞雪, 周晨曦, 杨慧敏, 雍兴跃, 刘景军 |
|
Microstructural Evolution and Dynamic Failure Mechanism of B10 Cu-Ni Alloy Under Multiple Stress Coupling in Flowing Seawater |
| LI Ruixue, ZHOU Chenxi, YANG Huimin, YONG Xingyue, LIU Jingjun |
| 图4 不同海水压力下(海水流速为0) B10合金腐蚀10 h前后的SEM像、XRD谱、(111)晶面的微应变及位错密度 |
| Fig.4 SEM images of B10 alloy before (a) and after corrosion for 10 h under seawater pressures 0.1 MPa (b), 4.0 MPa (c), 6.0 MPa (d), 8.0 MPa (e), and 12.0 MPa (f); XRD patterns (g); microstrains of (111) crystal plane (h); and dislocation density of (111) crystal plane (i) at a seawater flow rate of 0 |
|