基于机器学习与多目标优化的304L不锈钢激光粉末床熔融工艺优化研究
徐青青, 闫震, 郭玉玉, 侯娟, 王皞, 黄爱军

Research on Optimization of Laser Powder Bed Fusion Process for 304L Stainless Steel Based on Machine Learning and Multi-Objective Optimization
XU Qingqing, YAN Zhen, GUO Yuyu, HOU Juan, WANG Hao, HUANG Aijun
图15 S1和S2试样显微组织的SEM像
Fig.15 Low and high (insets) magnified SEM images of S1 sample processed at 220 W (a) and S2 sample processed at 278 W (b)