基于机器学习与多目标优化的304L不锈钢激光粉末床熔融工艺优化研究
徐青青, 闫震, 郭玉玉, 侯娟, 王皞, 黄爱军

Research on Optimization of Laser Powder Bed Fusion Process for 304L Stainless Steel Based on Machine Learning and Multi-Objective Optimization
XU Qingqing, YAN Zhen, GUO Yuyu, HOU Juan, WANG Hao, HUANG Aijun
图12 基于NSGA-II-TOPSIS算法获得的解集(其中TOPSIS为逼近理想解排序法)
Fig.12 Pareto front distribution identified by NSGA-II (a) and optimal solution identified by the TOPSIS (b) (TOPSIS—technique for order preference by similarity to ideal solution. S1, S2, and S3—three process parameters)