基于机器学习与多目标优化的304L不锈钢激光粉末床熔融工艺优化研究
徐青青, 闫震, 郭玉玉, 侯娟, 王皞, 黄爱军

Research on Optimization of Laser Powder Bed Fusion Process for 304L Stainless Steel Based on Machine Learning and Multi-Objective Optimization
XU Qingqing, YAN Zhen, GUO Yuyu, HOU Juan, WANG Hao, HUANG Aijun
图7 各模型基于Monte Carlo交叉验证(MCCV)的50 cyc独立重复实验所得测试集性能箱型图对比
Fig.7 Boxplot comparisons of testing set performances of different models based on 50 cyc independent MCCV trials (Points represent outliers, boxes represent interquartile range (IQR))
(a-c) R2 distributions for UTS (a), YS (b), and EL (c)
(d-f) MAE distributions for UTS (d), YS (e), and EL (f)