超高强度钢析出相调控与强化机理研究现状及发展趋势
张朝磊, 潘晓坤, 高军恒, 吴宏辉, 毛新平

Research Status and Development Trend of Precipitation Phase Regulation and Strengthening Mechanism in Ultra-High Strength Steel
ZHANG Chaolei, PAN Xiaokun, GAO Junheng, WU Honghui, MAO Xinping
图7 新型超高强度钢中典型复合析出相的析出机制[91,92,94,95]
Fig.7 Precipitation mechanisms of typical composite precipitates in novel ultra-high strength steels
(a) Cu/NiAl[91] (b) B2-NiAl/η-Ni3Ti[92] (c) B2-NiAl/L21-Ni2TiAl[94] (d) NiMn/Ni2AlMn[95]