Nb稳定化奥氏体不锈钢在第四代核电领域的研究进展 |
| 陈胜虎, 谢昂, 杨彬彬, 刘涌涛, 陈思含, 赵明久, 姜海昌, 戎利建 |
|
Research Progress of the Niobium-Stabilized Austenitic Stainless Steels for Generation-IV Nuclear Reactors |
| CHEN Shenghu, XIE Ang, YANG Binbin, LIU Yongtao, CHEN Sihan, ZHAO Mingjiu, JIANG Haichang, RONG Lijian |
| 图10 NbC/基体界面捕获点缺陷的微观机制[ |
| Fig.10 Schematic illustration of the 3D structure after irradiation (a) and evolution of irradiation-induced defects along the NbC/matrix interface (b)[ |
|