Nb稳定化奥氏体不锈钢在第四代核电领域的研究进展 |
| 陈胜虎, 谢昂, 杨彬彬, 刘涌涛, 陈思含, 赵明久, 姜海昌, 戎利建 |
|
Research Progress of the Niobium-Stabilized Austenitic Stainless Steels for Generation-IV Nuclear Reactors |
| CHEN Shenghu, XIE Ang, YANG Binbin, LIU Yongtao, CHEN Sihan, ZHAO Mingjiu, JIANG Haichang, RONG Lijian |
| 图9 Nb添加对Fe-16Ni-15Cr合金50 dpa离子辐照条件下空洞密度和直径的影响[ |
| Fig.9 Variation in void number density (a) and mean void diameter (b) in Fe-16Ni-15Cr and Fe-16Ni-15Cr-0.6Nb alloys after irradiation to 50 dpa[ |
|