Nb稳定化奥氏体不锈钢在第四代核电领域的研究进展 |
| 陈胜虎, 谢昂, 杨彬彬, 刘涌涛, 陈思含, 赵明久, 姜海昌, 戎利建 |
|
Research Progress of the Niobium-Stabilized Austenitic Stainless Steels for Generation-IV Nuclear Reactors |
| CHEN Shenghu, XIE Ang, YANG Binbin, LIU Yongtao, CHEN Sihan, ZHAO Mingjiu, JIANG Haichang, RONG Lijian |
| 图7 316L钢和Nb稳定化20Cr25Ni奥氏体不锈钢的温度-时间-析出(TTP)曲线[ |
| Fig.7 Temperature-time-precipitation phase diagrams of 316L steel (a)[ |
|