Nb稳定化奥氏体不锈钢在第四代核电领域的研究进展 |
| 陈胜虎, 谢昂, 杨彬彬, 刘涌涛, 陈思含, 赵明久, 姜海昌, 戎利建 |
|
Research Progress of the Niobium-Stabilized Austenitic Stainless Steels for Generation-IV Nuclear Reactors |
| CHEN Shenghu, XIE Ang, YANG Binbin, LIU Yongtao, CHEN Sihan, ZHAO Mingjiu, JIANG Haichang, RONG Lijian |
| 图3 铸态试样中初生NbC和奥氏体的纳米压痕结果及室温变形后组织形貌的TEM像[ |
| Fig.3 Nanoindentation load-depth curves of primary NbC and austenite (a) and TEM images near primary NbC after deformation to a true strain of 10% (b) in as-cast sample (SF—stacking fault. Inset in Fig.3b refers to the corresponding SAED pattern of NbC)[ |
|