Nb稳定化奥氏体不锈钢在第四代核电领域的研究进展
陈胜虎, 谢昂, 杨彬彬, 刘涌涛, 陈思含, 赵明久, 姜海昌, 戎利建

Research Progress of the Niobium-Stabilized Austenitic Stainless Steels for Generation-IV Nuclear Reactors
CHEN Shenghu, XIE Ang, YANG Binbin, LIU Yongtao, CHEN Sihan, ZHAO Mingjiu, JIANG Haichang, RONG Lijian
图2 Nb含量对Fe-15Cr-10Ni奥氏体不锈钢中NbC析出行为的热力学模拟计算与含0.9%Nb铸态组织的OM像
Fig.2 Thermo-Calc calculation of NbC formation in Fe-15Cr-10Ni ausenitic stainless steels with different Nb contents (a) and OM image of as-cast samples with 0.9%Nb (b) (Inset in Fig.2b is the high magnification image of the primary NbC)