轨道交通用SiCp 增强铝基复合材料制动盘研究与应用进展 |
||||||||||||||||||
| 谭东, 吴刘坤, 付康习, 夏少华, 李冲, 崔雷, 刘永长, 昝宇宁 | ||||||||||||||||||
|
Research and Application Progress of SiCp-Reinforced Aluminum-Based Composite Brake Discs for Rail Transit Vehicles |
||||||||||||||||||
| TAN Dong, WU Liukun, FU Kangxi, XIA Shaohua, LI Chong, CUI Lei, LIU Yongchang, ZAN Yuning | ||||||||||||||||||
| 表2 列车制动盘牵引能耗计算[ |
||||||||||||||||||
| Table 2 Traction energy consumption calculation for a Train's brake discs[ |
||||||||||||||||||
|
||||||||||||||||||