轨道交通用SiCp 增强铝基复合材料制动盘研究与应用进展 |
||||||||||||||||
| 谭东, 吴刘坤, 付康习, 夏少华, 李冲, 崔雷, 刘永长, 昝宇宁 | ||||||||||||||||
|
Research and Application Progress of SiCp-Reinforced Aluminum-Based Composite Brake Discs for Rail Transit Vehicles |
||||||||||||||||
| TAN Dong, WU Liukun, FU Kangxi, XIA Shaohua, LI Chong, CUI Lei, LIU Yongchang, ZAN Yuning | ||||||||||||||||
| 表1 铝基复合材料制动盘盘体材料力学性能对比(实测平均值) |
||||||||||||||||
| Table 1 Comparisons of mechanical properties (measured average values) of aluminum-based composite brake-disc body materials |
||||||||||||||||
|
||||||||||||||||