激光粉末床熔融镍基高温合金中第二相演化机制与调控策略进展 |
| 彭望君, 王长河, 杜大帆, 董安平, 陈彪, 孙宝德 |
|
A Review on the Evolution Mechanisms and Regulation Strategies of Secondary Phases in Laser Powder Bed Fusion Nickel-Based Superalloys |
| PENG Wangjun, WANG Changhe, DU Dafan, DONG Anping, CHEN Biao, SUN Baode |
| 图4 第二相分布和相演化规律[ |
| Fig.4 Distribution and phase evolution laws of the secondary phase (a) oxide distribution[ (b) phase transformation during heat treatment[ (c) phase transformation during solid solution-aging heat treatment[ (d) in situ oxide formation[ |
|