通过非金属小原子间隙填充调控高熵薄膜的局域化学序与多种性能:逾渗理论视角
李晓娜, 王箫, 王达哲, 郑月红, 董闯, P. K. LIAW

Tuning Local Chemical Order and Multiple Properties in High-Entropy Films via Interstitial Filling with Non-Metallic Small Atoms: A Percolation- Theory-Based Perspective
LI Xiaona, WANG Xiao, WANG Dazhe, ZHENG Yuehong, DONG Chuang, P. K. LIAW
表1 不同晶格体系逾渗阈值与配位数和堆积密度的关系[33]
Table 1 Relationships among percolation threshold, coordination number (z), and filling factor (v) in different crystal lattice systems[33]
Structurezvpcsitepcbondz·pcbondv·pcsite
fcc120.74050.1980.1191.430.147
bcc80.68020.2450.1791.430.167
Simple cubic60.52360.3110.2471.480.163
Diamond40.34010.4280.3881.550.146