通过非金属小原子间隙填充调控高熵薄膜的局域化学序与多种性能:逾渗理论视角 |
| 李晓娜, 王箫, 王达哲, 郑月红, 董闯, P. K. LIAW |
|
Tuning Local Chemical Order and Multiple Properties in High-Entropy Films via Interstitial Filling with Non-Metallic Small Atoms: A Percolation- Theory-Based Perspective |
| LI Xiaona, WANG Xiao, WANG Dazhe, ZHENG Yuehong, DONG Chuang, P. K. LIAW |
| 图7 La(Cr0.2Mn0.2Fe0.2Co0.2Ni0.2)O3薄膜在不同Mn含量下的磁滞回线与交换偏置场的变化,以及对应的Monte Carlo模拟展现了铁磁(FM)与反铁磁(AFM)交换作用逾渗网络的演变[ |
| Fig.7 Magnetic hysteresis loops and the variation of exchange bias field in La(Cr0.2Mn0.2Fe0.2Co0.2Ni0.2)O3 films with different Mn contents (a-c); and corresponding Monte Carlo simulation results, showing the evolution of percolating networks for FM (red) and AFM (blue) exchange interactions, where the color depth represents the magnetic exchange interaction strength (d-f)[ |
|