通过非金属小原子间隙填充调控高熵薄膜的局域化学序与多种性能:逾渗理论视角 |
| 李晓娜, 王箫, 王达哲, 郑月红, 董闯, P. K. LIAW |
|
Tuning Local Chemical Order and Multiple Properties in High-Entropy Films via Interstitial Filling with Non-Metallic Small Atoms: A Percolation- Theory-Based Perspective |
| LI Xiaona, WANG Xiao, WANG Dazhe, ZHENG Yuehong, DONG Chuang, P. K. LIAW |
| 图6 La(Cr0.2Mn0.2Fe0.2Co0.2Ni0.2)O3薄膜不同元素之间多样的磁交换作用、磁滞回线以及多层膜的交换偏置[ |
| Fig.6 Diverse magnetic exchange interactions between different elements in the La(Cr0.2Mn0.2Fe0.2Co0.2Ni0.2)O3 (L5BO) film (a), magnetic hysteresis loops of the L5BO film (b), and exchange bias in the L5BO/LSMO multilayer on STO (001) (c)[ |
|