通过非金属小原子间隙填充调控高熵薄膜的局域化学序与多种性能:逾渗理论视角
李晓娜, 王箫, 王达哲, 郑月红, 董闯, P. K. LIAW

Tuning Local Chemical Order and Multiple Properties in High-Entropy Films via Interstitial Filling with Non-Metallic Small Atoms: A Percolation- Theory-Based Perspective
LI Xiaona, WANG Xiao, WANG Dazhe, ZHENG Yuehong, DONG Chuang, P. K. LIAW
图4 (TiNbZr)86O12C1N1薄膜经原子探针层析呈现的元素分布及沿所示箭头方向的一维成分分布,微柱压缩的工程应力-应变曲线,以及通过悬臂梁弯曲测得的载荷-位移曲线[45]
Fig.4 Atom probe tomography elemental mapping of (TiNbZr)86O12C1N1 film (a), one-dimensional compositional profile along the arrow direction in Fig.4a (b), engineering stress-strain curves from microcompression testing (c), and load-displacement curves measured via cantilever beam bending (d)[45] (Inset in Fig.4c shows the O-12 massive interstitial solid solution (MISS) alloy pillar prior to compression; inset in Fig.4d shows the position of the diamond indenter tool, deforming the O-12 cantilever)