Al掺杂对CuInTe2热电性能的影响 |
| 杨二阔, 张泽宇, 王亚松, 彭威, 历长云, 李广书, 康慧君, 王同敏 |
|
Influence of Al Doping on Thermoelectric Properties of CuInTe2 |
| YANG Erkuo, ZHANG Zeyu, WANG Yasong, PENG Wei, LI Changyun, LI Guangshu, KANG Huijun, WANG Tongmin |
| 图8 CuIn1-xAlxTe2 (x = 0、0.01、0.03、0.1、0.2和0.3)化合物的热电优值 |