Al掺杂对CuInTe2热电性能的影响
杨二阔, 张泽宇, 王亚松, 彭威, 历长云, 李广书, 康慧君, 王同敏

Influence of Al Doping on Thermoelectric Properties of CuInTe2
YANG Erkuo, ZHANG Zeyu, WANG Yasong, PENG Wei, LI Changyun, LI Guangshu, KANG Huijun, WANG Tongmin
图3 CuIn0.97Al0.03Te2样品纵截面和横截面的SEM像及EDS元素面分布图
Fig.3 SEM images and corresponding EDS element distribution mappings of longitudinal (a) and transverse (b) sections of CuIn0.97Al0.03Te2 sample