Al掺杂对CuInTe2热电性能的影响 |
| 杨二阔, 张泽宇, 王亚松, 彭威, 历长云, 李广书, 康慧君, 王同敏 |
|
Influence of Al Doping on Thermoelectric Properties of CuInTe2 |
| YANG Erkuo, ZHANG Zeyu, WANG Yasong, PENG Wei, LI Changyun, LI Guangshu, KANG Huijun, WANG Tongmin |
| 图2 CuIn1-xAlxTe2 (x = 0、0.01、0.03、0.1、0.2、0.3和0.5)粉末在303 K的XRD谱和(220)峰放大图 |
| Fig.2 XRD patterns of CuIn1-xAlxTe2 (x = 0, 0.01, 0.03, 0.1, 0.2, 0.3, and 0.5) powders at 303 K (a) and its enlargement of (220) peaks (b) |
|