带材厚度对Fe75.2Si13B8Cu1Nb2.8纳米晶软磁合金磁畴结构和高频磁性能的影响
施博文, 李艳辉, 冯拓, 王雨, 蒋丽, 于凤云, 杨陆, 张伟

Effect of Ribbon Thickness on Magnetic Domain Structures and High-Frequency Magnetic Properties of Fe75.2Si13B8Cu1Nb2.8 Nanocrystalline Soft Magnetic Alloy
SHI Bowen, LI Yanhui, FENG Tuo, WANG Yu, JIANG Li, YU Fengyun, YANG Lu, ZHANG Wei
图7 不同厚度Fe75.2Si13B8Cu1Nb2.8纳米晶带材的Pec和Pex与频率的关系
Fig.7 Frequency dependences of Pec (a) and Pex (b) of Fe75.2Si13B8Cu1Nb2.8 nanocrystalline ribbons with different thicknesses (Insets show the partial enlarged views of 10-100 kHz)