带材厚度对Fe75.2Si13B8Cu1Nb2.8纳米晶软磁合金磁畴结构和高频磁性能的影响 |
| 施博文, 李艳辉, 冯拓, 王雨, 蒋丽, 于凤云, 杨陆, 张伟 |
|
Effect of Ribbon Thickness on Magnetic Domain Structures and High-Frequency Magnetic Properties of Fe75.2Si13B8Cu1Nb2.8 Nanocrystalline Soft Magnetic Alloy |
| SHI Bowen, LI Yanhui, FENG Tuo, WANG Yu, JIANG Li, YU Fengyun, YANG Lu, ZHANG Wei |
| 图6 厚度为19 μm的Fe75.2Si13B8Cu1Nb2.8纳米晶带材的磁滞损耗(Ph)、涡流损耗(Pec)和剩余损耗(Pex)及各损耗占比(P / Pt)与频率的关系 |