带材厚度对Fe75.2Si13B8Cu1Nb2.8纳米晶软磁合金磁畴结构和高频磁性能的影响 |
| 施博文, 李艳辉, 冯拓, 王雨, 蒋丽, 于凤云, 杨陆, 张伟 |
|
Effect of Ribbon Thickness on Magnetic Domain Structures and High-Frequency Magnetic Properties of Fe75.2Si13B8Cu1Nb2.8 Nanocrystalline Soft Magnetic Alloy |
| SHI Bowen, LI Yanhui, FENG Tuo, WANG Yu, JIANG Li, YU Fengyun, YANG Lu, ZHANG Wei |
| 图5 843 K退火60 min后不同厚度Fe75.2Si13B8Cu1Nb2.8合金带材的XRD谱和TEM分析 |
| Fig.5 XRD patterns (a) and bright-field TEM images (Insets are SAED patterns and grain size distributions with normal fitting. N—normal distribution) (b-d) of Fe75.2Si13B8Cu1Nb2.8 alloy ribbons with different thicknesses after annealing at 843 K for 60 min (b) t = 15 µm (c) t = 19 µm (d) t = 23 µm |
|