带材厚度对Fe75.2Si13B8Cu1Nb2.8纳米晶软磁合金磁畴结构和高频磁性能的影响 |
| 施博文, 李艳辉, 冯拓, 王雨, 蒋丽, 于凤云, 杨陆, 张伟 |
|
Effect of Ribbon Thickness on Magnetic Domain Structures and High-Frequency Magnetic Properties of Fe75.2Si13B8Cu1Nb2.8 Nanocrystalline Soft Magnetic Alloy |
| SHI Bowen, LI Yanhui, FENG Tuo, WANG Yu, JIANG Li, YU Fengyun, YANG Lu, ZHANG Wei |
| 图3 不同厚度Fe75.2Si13B8Cu1Nb2.8合金带材的磁通密度(Bs)和矫顽力(Hc)与退火温度(Ta)的关系 |
| Fig.3 Variations in saturation magnetic flux density (Bs) (a) and coercivity (Hc) (b) of Fe75.2Si13B8Cu1Nb2.8 alloy ribbons with different thicknesses as a function of annealing temperature (Ta) |
|