带材厚度对Fe75.2Si13B8Cu1Nb2.8纳米晶软磁合金磁畴结构和高频磁性能的影响 |
| 施博文, 李艳辉, 冯拓, 王雨, 蒋丽, 于凤云, 杨陆, 张伟 |
|
Effect of Ribbon Thickness on Magnetic Domain Structures and High-Frequency Magnetic Properties of Fe75.2Si13B8Cu1Nb2.8 Nanocrystalline Soft Magnetic Alloy |
| SHI Bowen, LI Yanhui, FENG Tuo, WANG Yu, JIANG Li, YU Fengyun, YANG Lu, ZHANG Wei |
| 图2 厚度为23 µm的Fe75.2Si13B8Cu1Nb2.8快淬合金带材的TEM明场像、HRTEM像和选区电子衍射(SAED)花样 |
| Fig.2 Bright-field TEM (a) and HRTEM (b) images of melt-spun Fe75.2Si13B8Cu1Nb2.8 alloy ribbon with a thickness of 23 μm (Inset in Fig.2a is the corresponding SAED pattern) |
|