带材厚度对Fe75.2Si13B8Cu1Nb2.8纳米晶软磁合金磁畴结构和高频磁性能的影响
施博文, 李艳辉, 冯拓, 王雨, 蒋丽, 于凤云, 杨陆, 张伟

Effect of Ribbon Thickness on Magnetic Domain Structures and High-Frequency Magnetic Properties of Fe75.2Si13B8Cu1Nb2.8 Nanocrystalline Soft Magnetic Alloy
SHI Bowen, LI Yanhui, FENG Tuo, WANG Yu, JIANG Li, YU Fengyun, YANG Lu, ZHANG Wei
图1 不同厚度Fe75.2Si13B8Cu1Nb2.8快淬合金带材的XRD谱和差式扫描量热(DSC)曲线
Fig.1 XRD patterns (a) and DSC curves (b) of melt-spun Fe75.2Si13B8Cu1Nb2.8 alloy ribbons with different thicknesses (t—ribbon thickness, Tx1—onset temperature of the first crystallization peak, Tx2—onset temperature of the second crystallization peak)