基于有限元法探究实验条件对一种耐热钢压痕松弛行为的影响 |
| 武晓丹, 赵杰, 曹铁山, 陈家万, 林通, 张浩杰 |
|
Exploring the Influence of Experimental Conditions on Indentation Relaxation Behavior of a Heat-Resistant Steel Based on the Finite Element Method |
| WU Xiaodan, ZHAO Jie, CAO Tieshan, CHEN Jiawan, LIN Tong, ZHANG Haojie |
| 图14 两种压头在0.1 mm最大压深下的松弛曲线 |
| Fig.14 Relaxation curves of two indenters at 0.1 mm maximum pressure depth |
|