基于有限元法探究实验条件对一种耐热钢压痕松弛行为的影响
武晓丹, 赵杰, 曹铁山, 陈家万, 林通, 张浩杰

Exploring the Influence of Experimental Conditions on Indentation Relaxation Behavior of a Heat-Resistant Steel Based on the Finite Element Method
WU Xiaodan, ZHAO Jie, CAO Tieshan, CHEN Jiawan, LIN Tong, ZHANG Haojie
图13 Sanicro25钢在两种形状压头完全卸载后沿不同路径的等效塑性应变和等效蠕变应变分布曲线
Fig.13 Along different paths (a, d) on the specimen of Sanicro25 steel after unloading by two shapes of indenters, PEEQ (b, e) and CEEQ (c, f) distribution curves are shown (Insets in Figs.13c, e, and f are the locally enlarged diagrams)
(a-c) conical indenter (d-f) quadrangular pyramid indenter