基于有限元法探究实验条件对一种耐热钢压痕松弛行为的影响 |
| 武晓丹, 赵杰, 曹铁山, 陈家万, 林通, 张浩杰 |
|
Exploring the Influence of Experimental Conditions on Indentation Relaxation Behavior of a Heat-Resistant Steel Based on the Finite Element Method |
| WU Xiaodan, ZHAO Jie, CAO Tieshan, CHEN Jiawan, LIN Tong, ZHANG Haojie |
| 图3 Sanicro25钢在圆锥形压头和四棱锥形压头在最大压痕深度0.1 mm下的压痕模拟结果与实验结果对比 |
| Fig.3 Comparison of simulation and experimental results for Sanicro25 steel under conical (a) and quadrangular pyramid (b) indenters with a depth of 0.1 mm (F—maximum force, t—compression head pressing time) |
|