表2 图3a~c中位置1~6的EDS成分分析结果 (atomic fraction / %)
Table 2 EDS compositional analysis results for locations 1-6 in Figs.3a-c
LocationMgMnFeSiAlPhase
11.337.884.920.0285.74Al6(Mn, Fe)
24.620.430.1333.2161.60Mg2Si
39.180.050.0050.8439.90Mg2Si
40.977.915.380.0585.57Al6(Mn, Fe)
58.323.394.020.1584.05Al6(Mn, Fe)
610.660.160.0217.1172.05Mg2Si