5A06合金TIG焊接头敏化失效机制及还原调控
李维, 冯杰涛, 房灿峰, 冯肖, 高武, 刘敏, 王英敏

Sensitization Failure Mechanism and Reversion Regulation of TIG Welded Joints in 5A06 Alloy
LI Wei, FENG Jietao, FANG Canfeng, FENG Xiao, GAO Wu, LIU Min, WANG Yingmin
表1 基材和焊丝的化学成分 (mass fraction / %)
Table 1 Chemical compositions of base material and weld-ing wire
AlloyMgMnFeSiCuTiZnAl
5A066.120.720.190.060.020.030.01Bal.
5B066.450.610.160.050.020.180.01Bal.