5A06合金TIG焊接头敏化失效机制及还原调控 |
| 李维, 冯杰涛, 房灿峰, 冯肖, 高武, 刘敏, 王英敏 |
|
Sensitization Failure Mechanism and Reversion Regulation of TIG Welded Joints in 5A06 Alloy |
| LI Wei, FENG Jietao, FANG Canfeng, FENG Xiao, GAO Wu, LIU Min, WANG Yingmin |
| 图9 5A06合金焊接态、敏化及还原样品不同区域经NAMLT测试后截面形貌的OM像 |
| Fig.9 Cross-sectional OM images showing the intergranular corrosion propagation paths after NAMLT for as-welded (a, d, g, j); 175 oC, 100 h sensitized (b, e, h, k); 310 oC, 1 h short-term reversion treated (c, f, i); and 310 oC, 24 h long-term reversion treated (l) 5A06 alloy samples (Figs.9j and k show the enlarged images of Figs.9g and h, respectively) (a-c) BM (d-f) HAZ (g-l) WZ |
|